Skip to content

Foundry

From pattern to finished tooth

We are a manufacturer, not a reseller: every tooth, adapter and cutting edge is cast, heat treated and tested in our own foundry.

Molten steel flowing from a melting furnace in a foundry (representative image)

Process

Casting process step by step

  1. 01

    Pattern making

    Patterns and cores are made from OEM dimensions and customer samples; the tooth pocket is dimensioned to fit the adapter nose exactly.

  2. 02

    Moulding

    Casting moulds are prepared and cores placed; mould dimensions are checked before pouring.

  3. 03

    Melting & pouring

    Low-alloy CrMnSi or CrNiMo steel is melted; chemical composition is checked by spectrometer before pouring.

  4. 04

    Heat treatment

    Quenched at 850 – 930 °C + tempered at 190 – 250 °C, giving the tooth both wear resistance and toughness.

  5. 05

    Cleaning & testing

    After fettling and surface cleaning, surface and core hardness are measured and dimensions checked.

  6. 06

    Packing & shipping

    Products are coded and packed on pallets or in crates, ready for domestic and export shipment.

Wholesale & export quotes

Send your code, factory-direct quote

Write to us with an OEM code, system or a photo of the old tooth; we will identify the compatible product and send a quantity-based quote.