Quality
Material, hardness, tested
A good tooth balances hardness and toughness: hard enough to resist wear, tough enough not to crack. These are the values we work to.
Technical standards
| Material | Low-alloy CrMnSi / CrNiMo cast steel |
|---|---|
| Steel grades | 25CrMnSi · 30CrMnSi · 35CrMnSi · CrNiMo |
| Hardness | HRC 45 – 52 (≈ 430 – 520 HB) |
| Hardness measurement | Surface and core measured separately |
| Heat treatment | Quenched at 850 – 930 °C + tempered at 190 – 250 °C |
Tests and inspections
Spectrometer analysis
Chemical composition of every melt is checked before pouring.
Hardness testing
Surface and core hardness are measured separately (HB / HRC).
Charpy impact test
Toughness is verified so the tooth does not crack under impact.
Metallography
Microstructure is examined after heat treatment.
Ultrasonic & magnetic particle
Internal and surface defects are checked on critical parts.
Dimensional check
Pocket and pin hole dimensions are checked for a correct fit.
Test reports for a specific order can be requested with your quote.
FAQ
Frequently asked questions
01Why is a harder tooth not always better?
Beyond a point, higher hardness reduces toughness and the tooth can crack under impact. Rock and impact work needs a balanced hardness with verified Charpy values.
02What is the difference between HB and HRC?
Both are hardness scales: Brinell (HB) and Rockwell C (HRC). HRC 45 – 52 corresponds to roughly 430 – 520 HB.

Wholesale & export quotes
Send your code, factory-direct quote
Write to us with an OEM code, system or a photo of the old tooth; we will identify the compatible product and send a quantity-based quote.